2017年11月3日星期五

Methods to masonry of boiler castable

There are several methods could be taken, to protect the boiler castable from being destroyed during masonry.
(1) The balance of refractory castable and water is important, adding not too much or too little water.
(2) Blended castable should be used within 30 minutes, and please add it to the certain depth and length at a time.
(3) Mold of it could be demolished after the castable is strong enough. The load-bearing form should be demolished when the castable reaches 70% of the strength. In order to facilitate stripping, pouring all the mold before pouring surface should be coated with a layer of oil.
(4) After the boiler masonry to have enough natural drying period, so that most of the refractory layer of water can be precipitated.
(5) Before the oven, the furnace lining material must have a certain natural strength (enough safety period) to carry out. Oven principle "should not be short, should be slow should not be fast."
Changxing refractory provides refractory products, calcium silicate products, castable & mortar, china refractory brick, ceramic fiber felt, ladle & tundish nozzle, ceramic fiber with high quality for you. Such as high alumina refractory bricks, Magnesia Carbon Brick, clay refractory bricks and other refractory products.
Article Source: Methods to masonry of boiler castable
Company name: Henan Xinmi Changxing Refractory Materials Co.,Ltd
Email: sales1@chinafirebrick.com
Website:http://www.chinafirebrick.com/
Intermediate Frequency Induction Furnace Lining Material

没有评论:

发表评论