Factors Affecting Refractory Materials for Electric Furnace Cover

1.Arc radiation
When the electric furnace is smelted, the arc temperature generated by the discharge of the electrode is as high as 3000 ° C or more, and the small furnace cover working face is subjected to severe melting loss.
2.Thermal shock
The arc heating, tapping and the rotation of the furnace cover to the outside of the furnace cause quenching and rapid heat, which causes the furnace cover to generate thermal stress and cause the working surface to peel off.
3. Chemical attack
The molten steel and slag are sprayed onto the working surface of the furnace cover, and some of the chemical components chemically react with the working surface and penetrate into the working surface to form a metamorphic layer.
4. Electrode spray water
The use of spray water on the electrode not only reduces the electrode consumption, but also causes the temperature around the electrode hole to decrease, thereby suppressing the high temperature melt loss to some extent. If this measure is not used, the electrode hole damage will be aggravated, mainly as reaming.
Changxing refractory provides refractory products, calcium silicate products, castable & mortar, china refractory brick, ceramic fiber felt, ladle & tundish nozzle, ceramic fiber with high quality for you. Such as high alumina refractory bricksmagnesia carbon brick, clay refractory bricks and other refractory products.

Article Source : Factors Affecting Refractory Materials for Electric Furnace Cover
Company name:Henan Xinmi Changxing Refractory Materials Co.,Ltd
Email: sales1@chinafirebrick.com
Website:http://www.chinafirebrick.com/
electric furnace

没有评论:

发表评论